Inner Conductor
Material – CCS bonded to dielectric
Diameter -1.02mm

Dielectric 
Material – Foam PE
Diameter – 4.57m

Shielding
Foil – Aluminum / Polyester / Aluminum
Braid – Aluminum 40%-90% optional
Foil – N/A (STD) | Aluminum / Polyester / Aluminum (TRI, QUAD)
Braid – N/A (STD) | N/A (TRI) | Aluminum 40% (QUAD)

Sheath
Material – PVC | LSZH | PE
Diameter – 6.86mm (STD) | 6.93mm (TRI) | 7.49mm (QUAD)
Color – Black / White

Messenger Wire(Optional)
Material – Gavlvanized Steel
Diameter – 1.30mm / 1.83mm

Operating Temperature – -20℃ to 75℃
Jacket Spark Test Voltage – 2500V
Dielectric Withstand Voltage – 1500 VAC
Cable Impedence – 75 ohms
Capacitance 53 pF/m
Pulling Tension – 45lbs
Bend Radius(Install) – 76mm
Velocity of Propagation – 83%
Screening Attentuation (dB)
5MHz to 1000MHz – 85 (STD) | 105 (TRI) | 120 (QUAD)
1000MHz to 3000MHz –  65 (STD) | 75 (TRI) | 85 (QUAD)

Frequency (MHz) – 5 | 55 | 83 | 187 | 211 | 250 | 300 | 400 | 550
Attenuaiton (dB/100m) @20℃ – 1,90 | 5,25 | 6,40 | 9,35 | 10,00 | 10,82 | 11,64 | 13,61 | 16,08
Structural Return Loss ( dB ) – 23 | 20

Frequency (MHz) – 600 | 750 | 865 | 1000 | 1500 | 1800 | 2050 | 2200 | 3000
Attenuaiton (dB/100m) @20℃ – 16,83 | 18,34 | 20,01 | 21,49 | 26,50 | 28,90 | 31,04 | 32,80 | 39,00
Structural Return Loss ( dB ) – 20 | 18

EN50117,CPR, SCTE74, ETL(UL), ROHS, CE